Grade 2 titanium (UNS R50400) is commercially pure titanium: unalloyed, about 99.2% titanium minimum, with oxygen as the main controlled addition. It is the default grade for corrosion-resistant process equipment — heat exchanger tube, chemical vessels, linings, piping and marine hardware — wherever moderate strength is sufficient and resistance to chlorides matters more than high strength.
CP is not a purity claim in the precious-metal sense. The four commercially pure grades are all unalloyed titanium, separated mainly by oxygen and iron, and oxygen is what raises strength at the cost of ductility. Grade 2 sits in the middle: enough oxygen for a useful 345 MPa minimum tensile strength, still ductile enough to cold form, bend and weld. Typical limits per the ASTM product specifications are 0.25% oxygen max, 0.30% iron max, 0.03% nitrogen and 0.015% hydrogen, at a density of about 4.51 g/cm³.
The commercial case for GR2 is a passive oxide film that re-forms instantly when scratched, in environments where stainless steel either pits or needs an expensive super-austenitic grade:
Continuous service in air is typically quoted at around 300–400 °C for CP grades, application dependent.
Knowing the limits is what separates a correct grade call from an expensive field failure:
The choice is usually driven by strength requirement first, formability second:
| Grade | UNS | Typical annealed UTS / yield (MPa) | Where it fits |
|---|---|---|---|
| Grade 1 | R50250 | 240 / 170 | Maximum formability, linings, low-fin tube where fins are cold rolled |
| Grade 2 | R50400 | 345 / 275 | The general corrosion grade: heat exchanger tube, vessels, marine hardware |
| Grade 9 (Ti-3Al-2.5V) | R56320 | 620 / 483 | Tubing where strength-to-weight matters, hydraulic and instrument lines |
| Grade 5 (Ti-6Al-4V) | R56400 | 895 / 828 | Highest strength duty: airframe parts, pump and valve internals, fasteners |
These are typical minimum values from the relevant ASTM product specifications; the applicable specification, revision and acceptance criteria are confirmed on the purchase order, not inferred from a grade name. Grade 9 and Grade 5 buy strength with alloying — and with machining cost, since both cut harder than GR2.
Grade 2 comes in every mill form, each with its own product specification: ASTM B338 for seamless and welded tube (ASME SB-338 for pressure duty), B265 for sheet, strip and plate, B348 for bar, B363 for fittings and B381 for forgings. On the enquiry, state the grade with its UNS number, the product specification, condition (annealed is normal), size and tolerance class, test scope — hydrostatic or eddy current for tube, penetrant where welds or machined faces are involved — surface condition, and an EN 10204 3.1 mill test report tied to the heat number.
Buyers starting from the material side will find the grade background in what commercially pure titanium is, and the dimensional and standard choices in the titanium tube and pipe range.
FDtitanium supplies Grade 2 in tube, sheet, plate, bar and fittings, with production and inspection handled as one controlled release: incoming material verified by PMI against the mill certificate, tube tested by hydrostatic pressure and eddy current, and the document package issued with the shipment. MOQs run from a single trial length to production releases, lead time is quoted with the offer, and one accountable contact owns the order from drawing review to dispatch. Where the duty needs more strength than CP titanium gives, the Grade 5 (Ti-6Al-4V) overview explains the cost in machining and weldability.
It is one of the four commercially pure grades. All are unalloyed titanium; Grade 2 is the most widely used because it balances strength, ductility and weldability for corrosion service. Grade 1 is softer and more formable, Grades 3 and 4 progressively stronger and less ductile.
Yes — it is a standard material for seawater heat exchangers, desalination plant and marine piping. Two conditions need checking: crevices above roughly 70 °C, where crevice corrosion becomes possible, and cathodic protection systems, where hydrogen absorption should be reviewed for the operating temperature.
Considerably. Typical annealed minimums are around 345 MPa tensile for Grade 2 against 895 MPa for Grade 5 (Ti-6Al-4V). Grade 2 compensates with far better formability and weldability and lower machining cost, which is why it dominates corrosion-duty equipment rather than load-bearing structure.
For thin-section process equipment, generally not — the weld and heat-affected zone retain adequate ductility. Stress relief is considered for heavy sections, tight-tolerance machined assemblies or where the service environment is known to be aggressive, and the requirement should be written into the specification rather than left to the fabricator.