Titanium alloy density runs 4.43 to 4.51 g/cm³, about 43 percent lighter than steel and about 67 percent heavier than aluminium. Strength is where the argument turns: GR5 (Ti-6Al-4V) carries a minimum yield of 828 MPa, so per kilogram it holds roughly five times the load of ordinary structural steel.
That gap is real, and it is also conditional. Titanium wins on strength per unit mass, on temperature and on corrosion. It does not win on stiffness, and it does not win on price. Knowing which of those decides your part is the whole exercise.
Density alone tells you very little. Divide strength by density and the metals sort themselves into a different order.
| Material | Density (g/cm³) | Min yield (MPa) | Yield ÷ density (kN·m/kg) | Typical duty |
|---|---|---|---|---|
| GR2 (CP titanium) | 4.51 | 275 | 61 | Exchanger tube, chemical plant |
| GR9 (Ti-3Al-2.5V), annealed | 4.48 | 483 | 108 | Hydraulic and instrument tube |
| GR5 (Ti-6Al-4V) | 4.43 | 828 | 187 | Fittings, fasteners, pressure parts |
| Structural steel S275 | 7.85 | 275 | 35 | Frames, supports, general fabrication |
| Stainless 316L | 8.00 | 170 | 21 | Wet process pipework |
| Aluminium 6061-T6 | 2.70 | 276 | 102 | Light structures, housings |
Figures are typical minimums from the applicable product specification in the annealed or temper condition stated; density is nominal. The mill certificate for the lot governs.
Against steel the margin is wide and needs no qualifiers. GR5 yields 5.3 times as much load per kilogram as S275, and even unalloyed GR2 (commercially pure titanium) returns 1.7 times. That is why a titanium tube bundle can replace a steel one at a fraction of the weight without redesigning the support structure.
Against aluminium the picture is tighter than most sales sheets admit. GR5 beats 6061-T6 by about 1.8 times per kilogram, yet sits level with 7075-T6, the strongest common aerospace aluminium. So on specific strength alone, titanium does not outrun the best aluminium. What it does is hold that strength while aluminium softens, and resist chlorides while 7075 needs protection.
Young’s modulus for titanium is 105 to 120 GPa, for steel around 210 GPa, for aluminium around 69 GPa. Divide each by its density and all three land between 22 and 27 kN·m/kg. They are, in effect, equally stiff per kilogram.
Aluminium 6061-T6 loses much of its strength above about 150 °C, so its specific strength figure applies to a narrow band of service. GR2 holds useful strength to roughly 300 °C in air and GR5 to about 400 °C. Steel keeps strength higher still, up to the point where oxidation and creep take over, and pays for it with 43 percent more mass per unit volume.
Corrosion decides more specs than strength does. Titanium’s passive oxide film survives seawater and wet chlorides that force 316L into pitting and stress-corrosion cracking. Aluminium survives them only with coating or alloy selection. Thermal conductivity runs the other way: about 7 W/m·K for titanium against 50 for steel and 167 for aluminium, which is why titanium heat exchanger tube is specified thin-walled and often finned rather than plain.
Hydraulic lines are the clearest case. GR9 annealed yields 483 MPa at 4.48 g/cm³, and the same alloy in the cold worked and stress relieved condition reaches 725 MPa, so a thin wall carries the pressure and still bends, flares and welds on the shop floor. Aerospace hydraulic systems were built on that combination.
In a shell-and-tube exchanger, the wall is usually set by corrosion allowance, not hoop stress, so the density argument quietly disappears. GR2 does the work at lower cost. Integral low-fin tube follows the same logic: fins are cold-rolled from GR1 or GR2 commercially pure titanium because the metal has to flow, and typical fin counts, heights and surface-area ratios are quoted as reference only, with the actual configuration confirmed against the drawing and RFQ.
FDtitanium manufactures seamless and welded titanium tube to ASTM B338 and supplies bar to ASTM B348 and plate to ASTM B265, in GR2, GR5 and GR9. Every lot is identified by PMI against its mill certificate before release, and ships with an EN 10204 3.1 report. Hand-held XRF sorts the grades by alloy content but cannot read oxygen, so where chemistry has to be defended analytically, laboratories work against certified reference materials such as NIST SRM 654b. Trial quantities are accepted as a starting MOQ, and one contact owns the order from drawing review to dispatch.
If the decision comes down to price before properties, read the Grade 2 versus Grade 5 cost comparison next. Sizes, conditions and standards sit under titanium tube and pipe.
Yes, by about 43 percent at equal volume: 4.51 g/cm³ against 7.85 g/cm³. Against aluminium it is the heavier metal, by roughly 67 percent, which is why airframes still use aluminium where strength per kilogram is not the limiting factor.
Not in absolute terms. GR5 at 828 MPa minimum yield beats ordinary structural steel at 275 MPa, but quenched and tempered alloy steels reach 1,000 MPa and above. Titanium’s claim is strength per kilogram, where it leads steel by five times.
Because service conditions rule it out. Aluminium loses strength above about 150 °C, needs coating in chlorides and expands three times as much per degree. Titanium holds strength to 300 °C or beyond, survives seawater uncoated and sits closer to composite structures on thermal expansion.
No. Wall thickness comes from pressure, corrosion allowance, erosion and vibration. Density changes the mass of the finished tube, not the wall the calculation produces.
Send the medium, temperature, pressure, load path and any forming you plan, with sizes and quantities, to FDtitanium, a titanium tube manufacturer. The offer states grade, specification, condition, inspection scope and lead time, so it can be compared line for line with another mill’s quote.
© 2026. All Rights Reserved. Zhangjiagang FD Titanium Industries Co.,LTD